The general flotation method was developed by Havens. Deslimed chromite ore was floated at pH 1.5 to 5.5 using a long-chain fatty-acid collector and soluble fluoride ions as a silicate depressant. The Havens method was later modified slightly to permit flotation without preliminary desprm. 3.1 Chrome magnetic separation process The chrome ore